Refueler
Well-Known Member
It is generally accepted that you do not do GRP work Gel or laminating in less than 15C temperature - otherwise curing is seriously affected.
Depending on the polyester as well - many will stay 'tacky' on the surface as it oxidises and fails to set ... but underneath that very thin top film - its set ok. Clingfilm is the usual answer to it - but again if temp is low - no g'tee at all.
Depending on the polyester as well - many will stay 'tacky' on the surface as it oxidises and fails to set ... but underneath that very thin top film - its set ok. Clingfilm is the usual answer to it - but again if temp is low - no g'tee at all.