vyv_cox
Well-Known Member
I am interested in finding out why Deks Olje was a disaster?
The first problem was getting it on to the various vertical surfaces. It has the viscosity of water, making brushing it almost impossible without large numbers of runs down the topsides. Having succeeded, after an extremely long time considering the small area we were doing, we found that within a matter of weeks it was breaking down. After six months it was as if we had never done anything.
I suspect the problem to be that we were coating wood that had previously been varnished, so the Deks did not soak in. A new piece of timber that is used for hanging the outboard on the pushpit was done at the same time. After about ten years it is still in reasonable condition.