Good Morning all,
I’m calling on the worldly wisdom of ybw again. I need some advice on antifouling as I’ve never done it before.
This is the current condition of the hull:
The current antifouling is micron350 and for simplicity purposes I’m going to be redoing it with more of the same ?
From all the threads I’ve read everyone likes a simple job like me so the feeling seems to be just slap it on.
Hull has been pressure washed and this has cleaned it back well. My plan is to scrapany flakey bits off the get to work with the paint straight on top.
Does this sound okay? Given the condition do you think I need to prime with primocon or just crack on?
Once again thanks for the incoming advice, it’s appreciated.
Warren
I’m calling on the worldly wisdom of ybw again. I need some advice on antifouling as I’ve never done it before.
This is the current condition of the hull:
The current antifouling is micron350 and for simplicity purposes I’m going to be redoing it with more of the same ?
From all the threads I’ve read everyone likes a simple job like me so the feeling seems to be just slap it on.
Hull has been pressure washed and this has cleaned it back well. My plan is to scrapany flakey bits off the get to work with the paint straight on top.
Does this sound okay? Given the condition do you think I need to prime with primocon or just crack on?
Once again thanks for the incoming advice, it’s appreciated.