manifold
New Member
Hello.
I've recently bought a small aluminimum yacht (5083 2.6mm & 5mm) called an Extrovert 22. A few were made in the early 1980s.
Just wondered what people did who have owned these or other ally boats as part of care and maintenance for these type of hulls.
I'm particularly concerned with anode protection for electrolysis and galvanic corrosion as this boat will be used in a sea/river eastuary, albeit dry sailed from a dipping trailer. It does not appear to have ever had an anode fitted.
Also what preparations for antifoul as I am currently in the process of ripping all the coatings off below the waterline to enable thorough inspection. The first coat appears to be some kind of red paint rather than the atomic yellow etch primer I was expecting.
This one doesnt seem to have done too badly after 37 years with only light corrosion markings here and there where the paint has previously failed.
Thanks in advance.
David
I've recently bought a small aluminimum yacht (5083 2.6mm & 5mm) called an Extrovert 22. A few were made in the early 1980s.
Just wondered what people did who have owned these or other ally boats as part of care and maintenance for these type of hulls.
I'm particularly concerned with anode protection for electrolysis and galvanic corrosion as this boat will be used in a sea/river eastuary, albeit dry sailed from a dipping trailer. It does not appear to have ever had an anode fitted.
Also what preparations for antifoul as I am currently in the process of ripping all the coatings off below the waterline to enable thorough inspection. The first coat appears to be some kind of red paint rather than the atomic yellow etch primer I was expecting.
This one doesnt seem to have done too badly after 37 years with only light corrosion markings here and there where the paint has previously failed.
Thanks in advance.
David