lumphammer
Well-Known Member
We are having antifoul removed back to gel coat and keel blasted back to bare metal and then treated with Fertan.
I will be left with a lot of small holes to fill to get a smooth surface.
Should I fill and sand smooth and then prime or prime then fill the holes?
What is the best mix to do the filling? I am tempted by Chemical Metal filler but should probably use an epoxy with microfibres to bulk it out.
I will be left with a lot of small holes to fill to get a smooth surface.
Should I fill and sand smooth and then prime or prime then fill the holes?
What is the best mix to do the filling? I am tempted by Chemical Metal filler but should probably use an epoxy with microfibres to bulk it out.