Keith 66
Well-Known Member
Using polyester resin there is a limit to the amount of catalyst you can use, they say 1 to 2% & though you can use more it produces an weaker cure. At this time of the year you are pushing the boundaries of what is possible without heating, Infra red is most efficient.
To get a fast cure in winter without heating you can boost the resin prior to catalysing it with Cobalt accelerator, it must be mixed in well before you add the catalyst & you dont need much. Adding cobalt means that you can use polyester down to zero degrees or even below successfully without heating.
Roofing companies routinely use cobalt accelerator for working outside.
It is not that easy to get hold of today as if it comes into contact directly with Peroxide a nasty reaction often explosive occurs.
To get a fast cure in winter without heating you can boost the resin prior to catalysing it with Cobalt accelerator, it must be mixed in well before you add the catalyst & you dont need much. Adding cobalt means that you can use polyester down to zero degrees or even below successfully without heating.
Roofing companies routinely use cobalt accelerator for working outside.
It is not that easy to get hold of today as if it comes into contact directly with Peroxide a nasty reaction often explosive occurs.