NPMR
Well-Known Member
I have the 3-bladed fixed propellor off the boat at the moment.
Having scrubbed and polished it, there are 'stains' (like pitting - they're darker and don't polish out but aren't very pink) on the blades and around the centre boss, there are vaguely pinkisk stains as well.
But overall, the prop is 'brassy' and 'sings' when you tap it (i.e. not a dull sound) so I suspect it has some de-zincification (new anode and wiring put in last year, so can't be sure how good it was before that) but wanted opinions as to how far 'gone' it has to be before it should be binned.
Or who would/could look at it and give a sensible opinion, in deepest, darkest Cornwall!
Having scrubbed and polished it, there are 'stains' (like pitting - they're darker and don't polish out but aren't very pink) on the blades and around the centre boss, there are vaguely pinkisk stains as well.
But overall, the prop is 'brassy' and 'sings' when you tap it (i.e. not a dull sound) so I suspect it has some de-zincification (new anode and wiring put in last year, so can't be sure how good it was before that) but wanted opinions as to how far 'gone' it has to be before it should be binned.
Or who would/could look at it and give a sensible opinion, in deepest, darkest Cornwall!