Last winter I replaced my topmast forestay with new galvanised 3/4" circ. 7x7 wire as the original had been kinked. I coated it (as is my wont) with blacking consisting of equal parts of Stockholm Tar, Bitumastic and White Spirit. Halfway through the season the lower 6' was given another coat of blacking.
At the end of the season the stay was red rusty from top to bottom and in far worse condition than my shrouds (1" circ. 7x7, similarly coated each year) which had seen 11 season's use. I showed the stay to the chandlers from whom the wire had been obtained. Their comment was "it's all like that now-a-days" and offered to replace it with stainless steel.
I will be replacing my shrouds soon and I am reluctant to use stainless as (apart from the price) it does not splice as neatly and I believe Insurance Companies insist on its being scrapped after 10 years. Is decent galvanised wire no longer available?
At the end of the season the stay was red rusty from top to bottom and in far worse condition than my shrouds (1" circ. 7x7, similarly coated each year) which had seen 11 season's use. I showed the stay to the chandlers from whom the wire had been obtained. Their comment was "it's all like that now-a-days" and offered to replace it with stainless steel.
I will be replacing my shrouds soon and I am reluctant to use stainless as (apart from the price) it does not splice as neatly and I believe Insurance Companies insist on its being scrapped after 10 years. Is decent galvanised wire no longer available?