sequena1
Member
Two weeks ago I put the final coat of TOPLAC on my superstructure---( 2 undercoats --2 gloss, white on white grp) Inevitably I've got a few sags and less than perfect bits but overall I'm reasonably pleased with the result. However i believe one can improve the final finish by ?compacting? and polishing the paint. Could someone explain how you do this? How long to leave the paint to harden? Which are the good compounds to use etc? Also can anybody recommend a good polishing tool or are they all much the same? Presumably these small £20 car polishers are just not man enough for the job (32 ft motor-sailer and a chalky hull still to do!!!)
Would be extremely grateful for words of wisdom.
Would be extremely grateful for words of wisdom.