i have to ballast my keel which is 6mm mild steel. i need to source 3.5t of ballast. van de stadt recommends lead. it goes around £900 per ton. iron 180 per ton. now the questions are:
is it a normal practice to pour in melted lead and layer cast iron to save space?
if only pigs or ingots are being put in how would you treat mild steel before ballasting? this place i quite awkward to access(diameter of keel plate holes is around 150mm, it is going to be grit blasted where possible.
would you wax or epoxy for long term solution?
is it a normal practice to pour in melted lead and layer cast iron to save space?
if only pigs or ingots are being put in how would you treat mild steel before ballasting? this place i quite awkward to access(diameter of keel plate holes is around 150mm, it is going to be grit blasted where possible.
would you wax or epoxy for long term solution?